Delrin & POM Machining · Best Machinability, Low Friction & High Fatigue

Delrin & POM Acetal CNC Machining: Ultra-Low Friction & Tight Gears

High-precision Delrin CNC machining and POM acetal machining (±0.01mm) for low-friction gears, sliding latches, medical valve stems, and wear bushings.

Friction Coeff. (vs Steel)0.20 – 0.25 (Dry)
Water Absorption (24h)< 0.25% (Dimensional Lock)
Precision Hold±0.01 mm Repeatable
Homopolymer vs CopolymerDelrin 150 / POM-C / ESD

Machining Delrin (homopolymer POM-H) and copolymer acetal (POM-C) delivers the tightest repeatable CNC dimensional tolerances of all thermoplastics (±0.01 mm) thanks to negligible moisture absorption and brittle-free chip breaking. It is Jeton's go-to material for precision spur gears, camera gimbal bearings, travel-plug slide locks, and retractable leash ratchets.

Precision CNC machined white and black Delrin POM gears and low-friction bushings
Precision CNC machined white and black Delrin POM gears and low-friction bushings

POM / DELRIN Engineering Benchmark Profile

Machinability98/100
Dimensional Lock95/100
Low Friction90/100
Max Temp (100°C)55/100

Delrin (POM-H) vs. Acetal Copolymer (POM-C): Choosing the Right Rod Stock

Many buyers treat 'Delrin' and 'Acetal' as identical, yet thick homopolymer POM-H plates often harbor invisible centerline porosity inside slabs thicker than 40 mm. For thin heavy-load gears and snap latches under 25 mm thickness, DuPont Delrin (POM-H) gives 15% higher stiffness and fatigue life; for thick manifold blocks or hot-water/chemical contact above 60°C, copolymer POM-C eliminates centerline voids and prevents hydrolysis.

Engineering Advantages & Bonding Limits of Machined POM

  • Best-in-Class CNC Tolerance: Minimal hygroscopic swelling lets Jeton hold ±0.01 mm gear pitch and sliding clearance across humid shipping routes.
  • Zero Burr Clean Edges: Crisp chip shear cuts miniature gear modules, thin leaf springs, and sharp bearing shoulders without thermal smearing.
  • Low Adhesive Bondability Alert: Delrin is chemically inert—standard glues and paints do not stick. Rely on mechanical press-fits, knurled inserts, or ultrasonic welding.
  • Mold Transfer Parameters: When scaling to 86T–160T Haitian injection presses, we compensate for 1.8%–2.2% crystalline shrinkage with 85°C–95°C temperature-controlled molds.

Can Delrin & Acetal Be Injection Molded After CNC Validation?

Yes—100%. Once Delrin CNC functional tests confirm quiet gear meshing and spring endurance, Jeton designs single- or multi-cavity hardened molds (P20/S136) calibrated for POM's 1.8%–2.2% shrinkage.